Quick Details

  • Steel Grade: A286
  • Standard: AISI, ASTM, BS, DIN, GB, JIS
  • Dimensions: 1mm-2000mm
  • Place of Origin: Sichuan, China (Mainland)
  • Brand Name: CHUAN STEEL
  • Technique: Hot Rolled
  • Application: STAINLESS STEEL
  • Alloy Or Not: Is Alloy
  • Type: superalloy steel
  • GRADE: A286

Packaging & Delivery

Packaging Details in bundle
according to your requirement
Delivery Time about 30 days

Specifications

Round bar steel: 1mm to 2000mm
Square-shape steel: 50mm
stainless steel
GH2132/A286 superalloy steel

A286 / A-286   Specifications

Round bar steel: 1mm to 2000mm

Square-shape steel: 50mm  to  600mm

Plate steel:0.1mm  to  800mm

Width: 10mm to 1500mm

Length: We can supply any length based on the customer's requirement.

Forging: Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes

Tubings: OD: φ6-219 mm, with wall thickness ranging from 1-35 mm.

Finished goods condition: hot forging/hot rolling + annealing/normalizing + tempering/quenching + tempering

 

cold-rolled/ hot-rolled stainless steel sheet

 

A286 / A-286  

 

Carbon

--

0.08 max

Manganese

--

2.00 max

Silicon

--

1.00 max

Chromium

13.50

16.00

Nickel

24.00

27.00

Molybdenum

1.00

1.75

Iron

--

Balance

Titanium

1.90

2.10

Vanadium

0.10

0.50

Aluminum

--

0.35 max

Boron

0.003

0.010

 

Transaction History of the Supplier

Below is the information about the supplier's transactions conducted via Alibaba.com. If you require further details regarding the transaction data, please contact the supplier directly.

Transaction Overview

Transactions

Transaction Details

This supplier has completedtransactions with buyers from .

Shipping Destination
Transaction Value
Transaction Date
Email to this supplier
China (Mainland) | Trading Company
Supplier Assessments:
The supplier supports Trade Assurance – A free service that protects your orders from payment to delivery.
Supplier's Trade Assurance Limit: US $34,000
Learn More